Kevin,
I don't have a solution but I wonder if you've discussed the problem
with the solder manufacturers? They should understand the metallurgy of
their product and hopefully be able to give you a solution.
Regards,
Kevin Glidden wrote:
> You could try buying some composite material (pallet and fixture materials)
> and having replacement fingers machined for you..expensive solution but it
> would work...
>
> Kevin Glidden
> Manufacturing Engineer
> Luminescent Systems Inc.
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Neil Maloney
> Sent: Thursday, August 03, 2006 5:05 PM
> To: [log in to unmask]
> Subject: [TN] SAC 305 solder on TI wave solder machine transport fingers
>
> Greetings Technet.
>
> I have an interesting problem that has developed since we converted to our
> lead-free process. We have been using an Electrovert Astrapak for our wave
> solder operation for many years in our SnPb process. A few months ago, we
> converted the machine for SAC305 by installing new titanium parts
> (solderpot, pumps, wave guides, etc) and loaded it up with Alpha metals
> SAC305. We removed and cleaned up the transport fingers in alcohol while the
> pot conversion was under way. After putting the machine back together our
> new lead-free process seemed perfect -- except that now the SAC305 is
> sticking to the titanium transport fingers- I mean really sticking to them.
> The smooth wave doesn't seem to affect the fingers as much as the chip wave-
> but after a run of about 200 PCBs- the fingers are fouled with solder - to
> the point that we have to stop and brush out the fingers with a rotary wire
> brush.
>
>
> We never had this problem with leaded solder. We do not have an automatic
> finger-cleaner installed on the machine (we never had this problem before)
> and I cannot find one anywhere to retrofit. But the question still comes
> down to-- what is causing the solder to stick where it did not stick before?
>
>
> We use a no -clean flux (Alpha EF2202 or Indium 1075, makes no difference
> --the solder still sticks.) The fingers were not changed out (only soaked
> and cleaned with alcohol) when the rest of the machine was converted to
> lead-free.
>
> Any insight into solving the problem would be greatly appreciated.
>
> Neil Maloney, Manufacturing Engineer
> Contemporary Control Systems, inc
> 2431 Curtiss St Downers Grove, IL 60515
> (630) 963-7070 x132
> [log in to unmask]
> http://www.ccontrols.com <http://www.ccontrols.com/> http://www.ctrlink.com
> <http://www.ctrlink.com/>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please visit IPC web
> site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|