Well,
I guess that the same sort of cooling the pot down a bit to let the
formation of the copper IMC might work as well for the L-F alloys.
However, being the alloys less dense, the IMC may form on the bottom
of the solder pot, instead on the surface.
I imagine one should dig into the molten pot a little rake, or
something alike, and try to fetch them.
By the way, isn't there alloys made specifically up to balance the
solder in the pot?
I'm thinking of SAC300 or SN100CLe and Sn100CLe+, for example.
Ivan
Il giorno 31/ago/06, alle ore 15:39, Werner Engelmaier ha scritto:
> *This message was transferred with a trial version of CommuniGate
> (r) Pro*
> *This message was transferred with a trial version of CommuniGate
> (r) Pro*
> Hi Mike,
> I do not know of one either, and I think the much reduced density
> of SAC
> solders, in the absence of Pb, makes such a process unlikely.
>
> Werner
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16 for additional information, or contact Keach Sasamori
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|