An undesirable intermetallic formed during gold wire ball bonding on an
aluminum pad is generally referred to as "purple plague." This phase is
AuAl2.
Best regards,
Leo
NOTE: New address and phone:
Leo M. Higgins III, Ph.D.
Vice President, Engineering and Technology
ASAT, Inc.
13809 Research Blvd., Suite 635
Austin, Texas 78750
office phone 512-249-4758
mobile 512-423-2002
[log in to unmask]
www.asat.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Friday, July 07, 2006 2:37 AM
To: [log in to unmask]
Subject: Re: [TN] Corrosion on Gold plating
Hi Antonio,
The leads are brazed on this ceramic module, which means using of a high
temperature brazing material. The high temperature combined with the
colour makes me think of purple plague. Which means that gold and tin
has formed an intermetallic with that name, purple plague. If you
magnify the picture in shop, you can see that the purple is found on
nearly all the leads, close to the ceramic body. IF this is the fact, I
would not rely on such components, but reject them.
Another possibility is that purple plague has been created cause you
have run excessive current through the leads, but I find that scenario
less probable.
Before doing anything, I suggest you mold the part in acrylic or similar
plastic, grind until you reach a region near the ceramic body, polish
and study the cross section in a metallurgical microscope, even make
study in SEM.
I would also take another sample and make a bending test on the leads to
see what the brazing area is like. You bend 90 degrees in one direction,
bend back to zero, then another bend minus 90 degrees and back to zero.
Totally 180 degrees. If the leads fulfills that test without cracking or
loss of terminals, they are OK talking mechanical strength.
Ingemar Hernefjord
Ericsson Microwave Systems
Last working day, then holidays!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of antonio
Sent: den 6 juli 2006 15:46
To: [log in to unmask]
Subject: [TN] Corrosion on Gold plating
Please I have a lot of components with corrosion on terminals gold
plating. Please see picture. Could anyone suggest an acelerating test to
evaluate que problem?
thanks a lot
Antonio Souza
Brazil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|