Dear Mr. Krishnan,
Could you send any document or web site about
"DSC test to check the Tg of the material to see if it
fully cured" and "TMA test to see the T260C".
Thanks and best regards,
Nhan
----- Original Message -----
From: "Chezhian, Krishnan (Radhakrishnan)"
<[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, July 25, 2006 12:19 PM
Subject: Re: [TN] IPC webcast - Electroplating Technologies - 7/27/06
Hi Suresh,
The reason for delamination could be due to various causes. From the
description given below it is not clear whether you are able to see the
delamination or "popcorn" effect from the outer layers after your
outer-layer etch process or the delamination only occurs after the
boards have been subjected to a thermal excursion like HASL, thermal
shock, IR reflow or wave-solder process.
If the delamination is occurring over the copper surface on the
inner-layers, it is most probably the adhesion between the prepregs &
oxide-coated copper surface is poor. This could be due to poor or
insufficient oxide coating or the lamination parameters are not fine
tuned, so the material is not fully cured. Since you are saying both the
Isola & Nelco materials exhibit this phenomena, then it is most unlikely
to be a material issue.
You could run a DSC test to check the Tg of the material to see if it
fully cured or perform a TMA test to see the T260C, time to
delamination. If these numbers appear to be quite low than the vendors
spec. then you have an issue with the lamination processing parameters.
If you are seeing the delamination after the boards have been subjected
to a thermal excursion then there are other factors that would come to
play, like shelf life & storage conditions of the boards, how long the
boards have been kept & whether any baking was done prior to subjecting
to any thermal excursion, moisture absorption due to the hygroscopic
nature of the FR-4 material. Or if the boards have been subjected to a
Lead Free process & the laminate material used is not compatible to this
process etc.,
Pls provide more details as to the exact occurrence of the delamination
& we may be able to share more info on this........
Thanks & Best Regards,
Krishnan C
SANMINA-SCI
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of T Suresh Babu
Sent: Tuesday, July 25, 2006 11:53 AM
To: [log in to unmask]
Subject: Re: [TN] IPC webcast - Electroplating Technologies - 7/27/06
Dear Friends,
I am new member for Technet.We are experiencing the delamination in the
multilayer ten layer and above.We us Isola and Nelco prepeg we are
experiencing this problem with both materials.The delamination over the
copper area on innerlayer.We use black oxide for the innerlayer and
vacuum
press for lamination.
Can any one share your experience.
Regards
Suresh
----- Original Message -----
From: "Tina Nerad" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, July 25, 2006 2:39 AM
Subject: [TN] IPC webcast - Electroplating Technologies - 7/27/06
Electroplating technologies, including an overview of the plating
process and factors affecting plating distribution and throwing power,
are the topics in this webcast. Don't miss out on this opportunity to
learn everything you need to know about the electroplating process!
Electroplating Technologies
July 27th, 2006, 10:00 a.m. - 11:00 .am. (CDT)
To register for this webcast or for more information, visit:
http://www.ipc.org/calendar/2006/PWB_BasicWebcastSeries_0706/PWBFab_Webc
astSeries_706.htm
Following this webcast, IPC is hosting an in-depth workshop covering
every aspect of the PCB Manufacturing Process:
August 2, 2006, 8:00 a.m. - 4:30 p.m.
Bannockburn, IL
Instructor: Michael Carano
Electrochemicals, Inc.
To register for this workshop or for more information, visit:
http://www.ipc.org/calendar/2006/AdvTroubleshooting_0806/Advtroubleshoti
ng_806.htm
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
________________________________________________________________________
_____
Scanned by Sanmina-SCI eShield
________________________________________________________________________
_____
CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended only for use by
the addressee(s) named herein and may contain legally privileged and/or
confidential information. If you are not the intended recipient of this
e-mail message, you are hereby notified that any dissemination, distribution
or copying of this e-mail message, and any attachments thereto, is strictly
prohibited. If you have received this e-mail message in error, please
immediately notify the sender and permanently delete the original and any
copies of this email and any prints thereof.
ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS E-MAIL IS NOT
INTENDED AS A SUBSTITUTE FOR A WRITING. Notwithstanding the Uniform
Electronic Transactions Act or the applicability of any other law of similar
substance and effect, absent an express statement to the contrary
hereinabove, this e-mail message its contents, and any attachments hereto
are not intended to represent an offer or acceptance to enter into a
contract and are not otherwise intended to bind the sender, Sanmina-SCI
Corporation (or any of its subsidiaries), or any other person or entity.
_____________________________________________________________________________
Scanned by Sanmina-SCI eShield
_____________________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|