TECHNET Archives

July 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 11 Jul 2006 09:31:15 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Al Onderick <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Content-Transfer-Encoding:
7bit
From:
Al Onderick <[log in to unmask]>
Parts/Attachments:
text/plain (212 lines)
Can someone direct me to a picture of a blowhole in a older joint? Is this
seen from the surface or is cross sectioning or xray required?

-Al

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] On Behalf Of
[log in to unmask]
Sent: Wednesday, June 21, 2006 12:56 PM
To: [log in to unmask]
Subject: Re: [TN] Blowholes pandemic

Hi Ioan,


Have you tried and extend your soak time to allow the moisture to escape
prior to reaching the liquidus stage. I have seen this problem before and
slowing down the profile does help reduce this problem.


Best regards,


Gilbert Roberge
Technical Support Manager
Amtech Inc.
Ph: 800-435-0317
Fx: 203-481-5033
E-mail: [log in to unmask]



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Wednesday, June 21, 2006 11:54 AM
To: [log in to unmask]
Subject: Re: [TN] Blowholes pandemic

Multicore WS200 as WS and AIM NC254 as no-clean.

I want to state that both pastes work fine for us and publishing the
details
is not related to concerns about their performance.

Ioan

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stadem, Richard D.
Sent: Wednesday, June 21, 2006 11:41 AM
To: [log in to unmask]
Subject: Re: [TN] Blowholes pandemic


Ioan, which brand and part number solder paste are you using?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Wednesday, June 21, 2006 10:28 AM
To: [log in to unmask]
Subject: Re: [TN] Blowholes pandemic

One is ENIG with no-clean paste, the other one is HASL (with WS paste).

Thanks,

Ioan

-----Original Message-----
From: Lee parker [mailto:[log in to unmask]]
Sent: Wednesday, June 21, 2006 11:26 AM
To: TechNet E-Mail Forum; Tempea, Ioan
Subject: Re: [TN] Blowholes pandemic


Ioan

It may still be a board problem. I would bake some boards and assemble
some suspect parts. By the way, what board surface finish are you using?

Best regards

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389


----- Original Message -----
From: "Tempea, Ioan" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, June 21, 2006 8:56 AM
Subject: [TN] Blowholes pandemic


Hi Technos,

for a couple of days I see occurences of blowholes in the joints of,
guess
what, SMT 0603 resistors.

The reflow recipe did not change and we're talking about 2 different
established products, we have run many of each before. One is WS, the
other
one no-clean. Each one uses different brand of solder paste, SnPb.

I have changed the paste with fresh one, no positive results. I have
changed
the reels with different date codes, Bingo! But even the "bad" parts
were
quite fresh, less than one year old. One of them is pure Sn plated,
don't
know about the other ones.

The question is: where on Earth can humidity stay in a ceramic resistor?

What else can be the cause of the blowholes? Did not bake the boards,
since
changing the components worked, so I guess the PCBs are out of the
hook...

Thanks,

Ioan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2