Something Mechanical, I like that...
Thanks guys, now I know "Bai Si" is White, I'll have to look up orange
in chinese...LOL
Rodney
-----Original Message-----
From: R Sedlak [mailto:[log in to unmask]]
Sent: Monday, July 24, 2006 2:04 PM
Subject: Re: Whats a good way to verify material is Ti vs Stainless?
Nice, elegant, cheap... nicely done.
Rudy Sedlak
Martin Butcher <[log in to unmask]> wrote: If memory serves, Ti
gives off white sparks when touched to a grinding wheel. SS sparks
should be orange.
Granted its cheap and dirty, but hey...
Martin
-----Original Message-----
From: R Sedlak [mailto:[log in to unmask]]
Sent: Monday, July 24, 2006 10:14 AM
To: [log in to unmask]
Subject: Re: [TN] Whats a good way to verify material is Ti vs
Stainless?
Can you get known samples of Ti and SS?
I do not know for sure, but suspect strongly that a dilute (say 1% to
5%) solution of Ammonium Bifluoride would not attack SS rapidly enough
to be noticed, but would attack Ti rapidly enough to cause visible
bubbling, when it was dripped on a surface.
Try this out first, to see if my suspicions are correct.
Rudy Sedlak
RD Chemical Company
Rodney Miller wrote: Houston, we have a problem,
we are fighting a contaminated solderpot,
and I'm not finding the source... the machine is in China, so I'd
appreciate some test that I could convey which would tell me I'm not
losing my mind... yet
Rodney L. Miller
Tri-onics Inc
Highland / Shanghai
Integrity and Solutions for Electronic Outsourcing
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
How low will we go? Check out Yahoo! Messenger's low PC-to-Phone call
rates.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
Do you Yahoo!?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Everyone is raving about the all-new Yahoo! Mail Beta.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|