Drying the parts in an oven to shorten the drying time might solve that.
One of our local shops uses Dawn dish liquid.
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Kallin, Dan
Sent: Tuesday, July 11, 2006 1:29 PM
To: [log in to unmask]
Subject: Re: [LF] Simple Green
I have heard favorable review from machine shops using simple green with
one caveat - Rust.
Dan Kallin
Phone: 978.371.4155 Fax: 978.371.2468
Mobile: 978.760.0779
[log in to unmask]
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Liz Harriman
Sent: Tuesday, July 11, 2006 12:28 PM
To: [log in to unmask]
Subject: Re: [LF] Simple Green
In addition to the performance information that Pam pointed out on
TURI's
lab testing website, note that many Simple Green products (including
Crystal Simple Green) include 2-butoxyethanol (also called Butyl
Cellosolve
or ethylene glycol monobutyl ether). There is some evidence of high
chronic exposures causing reproductive toxicity, although that evidence
is
not conclusive, and there are other health cautions.
http://www.cdc.gov/niosh/ipcsneng/neng0059.html
It has a good environmental profile, so would be a good choice for boat
cleaning! It also may be considerably safer than what you are now using
to
remove mineral oils from parts.
Simple Green/Sunshine Makers, Inc. has good MSDS sheets that are readily
available on their web site.
http://industrial.simplegreen.com/ind_prod_cry.php
Liz Harriman
At 08:22 AM 7/11/2006 -0400, you wrote:
>The Toxics Use Reduction Institute's Surface Solutions Laboratory has
>been working with industry for over a decade identifying safer,
>non-toxic alternative cleaners for specific industrial needs. Jason
>Marshall, Laboratory Testing Manager at TURI's Lab, has created a
>database of cleaners, including Simple Green products, and associated
>cleaning needs. You can see this database at www.cleanersolutions to
>find out what kind of testing the TURI Lab has done for this product.
>
>Jason has found that the Simple Green products are acceptable for very
>light oils. Anything more than that and the cleaners aren't as
effective.
>--
>
>*Pam Civie*
>
>Industry Research Program Manager
>
>Toxics Use Reduction Institute
>
>University of Massachusetts Lowell
>
>1 University Ave, Lowell, MA 01854
>
>
>
>978-934-3142 978-934-3050 (fax)
>
>
>
>Visit our website at www.turi.org <http://www.turi.org/>
>
>
>
>
>
>
>
>/"//Ask not what the world needs. Ask what makes you come alive ...
>then go do it.
>Because what the world needs is people who have come alive."//
>/Howard Thurman
>
>
>
>
>
>Visit www.innerharmonymusic.com <http://www.innerharmonymusic.com/>
>
>*/Inner Harmony Music/* ... */a non-profit organization creating
>opportunities for healing and inner growth through sound/*
>
>
>-----------------------------------------------------------------------
--------Leadfee
>Mail List provided as a service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text
in
>the BODY (NOT the subject field): SIGNOFF Leadfree
>To temporarily stop/(start) delivery of Leadree for vacation breaks
send:
>SET Leadfree NOMAIL/(MAIL)
>Search previous postings at: http://listserv.ipc.org/archives
>Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask]
or
>847-615-7100 ext.2815
>-----------------------------------------------------------------------
--------
********************************************
Liz Harriman
Deputy Director
Massachusetts Toxics Use Reduction Institute
www.turi.org
University of Massachusetts Lowell
One University Ave
Lowell, MA 01854
Phone: 978-934-3387 Fax: 978-934-3050
*********************************************
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|