Hi Cheryl
Our plating shop uses
Entek Plus 106 A ( X )
which goes only onto copper and not an Au, Sn and other metal surfaces.
Our customers are successfull using such kind of boards.
--
Herbert W. Kruschitz
QSM (EOQ)
Senior Project Manager
OPTIPRINT AG
Auerstr. 37
CH-9442 Berneck
Tel : +41 (0)71 747 86 27
Cell: +41 (0)79 614 74 56
Fax : +41 (0)71 747 86 87
Mail: mailto:[log in to unmask]
URL: www.optiprint.ch
-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Cheryl Johnson
Gesendet: Donnerstag, 6. Juli 2006 20:42
An: [log in to unmask]
Betreff: [TN] osp over gold bond pads
Does any one have any experience they care to share with OSP over electroplated gold bond pads (on FLEX)?
It would save us 5 cents each if the gold pads didn't have to be masked before the OSP is applied...
Thank you for your help!
Sincerely,
-----------------------------------
Cheryl Johnson, C.I.D.+
Manager
ExcelStor US Office, Engineering Services
Email: [log in to unmask]
Tel: (303) 684-7291
Fax: (303) 684-7268
Mobile: (303) 809-5815
-----------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|