Hi Cheryl,
I can't speak to the wire bonding, but I do know that some OSP's bring
Copper into solution which allows the OSP to bond to the Gold. On
occasion, the OSP coating on the Gold CAN be enough to enough to prevent
electrical contact between an edge connector and socket. There exists
OSP formulations that do NOT coat the Gold plating. So with the right
formulation, it might be possible. Otherwise, buyer beware!
-Ryan Grant
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cheryl Johnson
Sent: Thursday, July 06, 2006 12:42 PM
To: [log in to unmask]
Subject: [TN] osp over gold bond pads
Does any one have any experience they care to share with OSP over
electroplated gold bond pads (on FLEX)?
It would save us 5 cents each if the gold pads didn't have to be masked
before the OSP is applied...
Thank you for your help!
Sincerely,
-----------------------------------
Cheryl Johnson, C.I.D.+
Manager
ExcelStor US Office, Engineering Services
Email: [log in to unmask]
Tel: (303) 684-7291
Fax: (303) 684-7268
Mobile: (303) 809-5815
-----------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|