Can you get known samples of Ti and SS?
I do not know for sure, but suspect strongly that a dilute (say 1% to 5%) solution of Ammonium Bifluoride would not attack SS rapidly enough to be noticed, but would attack Ti rapidly enough to cause visible bubbling, when it was dripped on a surface.
Try this out first, to see if my suspicions are correct.
Rudy Sedlak
RD Chemical Company
Rodney Miller <[log in to unmask]> wrote: Houston, we have a problem, we are fighting a contaminated solderpot,
and I'm not finding the source... the machine is in China, so I'd
appreciate some test that I could convey which would tell me I'm not
losing my mind... yet
Rodney L. Miller
Tri-onics Inc
Highland / Shanghai
Integrity and Solutions for Electronic Outsourcing
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
How low will we go? Check out Yahoo! Messenger’s low PC-to-Phone call rates.
|
|
|