No. On the parts that you are currently using the unused ball will
simply reflow and re-solidify to its BGA pad. It should not be a
problem. I would not attempt to remove the unused ball from the BGA
beforehand, just leave it be.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Black, Paul
Sent: Monday, July 17, 2006 11:03 AM
To: [log in to unmask]
Subject: [TN] BGA Pad Missing on Board
Hi Everyone,
I have a quick question on BGA's. I have a board that is laid out for a
BGA that the manufacturer is still developing. In the meantime, it can
be populated with a different BGA from the same manufacturer and
functionally it works fine. My problem is that the board layout has a
location where there is no BGA pad. The newer part has no ball in that
area but the one I am currently using does have a ball there. Are there
any potential problems of having a BGA ball reflowing but not having a
pad to bond with?
Thank you,
Paul Black
Manufacturing Engineer
Kronos
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|