TECHNET Archives

July 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Date:
Fri, 14 Jul 2006 13:42:48 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (118 lines)
Phew... the stripping issues you generate doing this must be incredible.

We had a photoresist stripper we dubbed "MND"... for "Minor Nuclear Device".
Sounds like you would need it after this treatment...

Rudy Sedlak
RD Chemical Company

Jeffrey Bush <[log in to unmask]> wrote: You can also do a 170F/15 Min bump in an oven to improve adhesion of DF to copper.

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
           76 Technology Drive - POB 1890
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 21
                    Fax - 802.257.0011


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak
Sent: Thursday, July 13, 2006 10:57 AM
To: [log in to unmask]
Subject: Re: [TN] Surface Roughness

Yusef Gimec:

  You bring up an interesting question.   With more modern dryfilm, it has been shown unnecessary for the copper to be roughened at all... in fact there is a related industry, the photochemical machining industry, which makes lead frames, which cannot tolerate any roughening, and uses dryfilms for etching copper.   We have developed cleaners for this industry, which clean the copper, but leave it shiney, and the dryfilm adheres very well.

  This ability to bond to a smooth surface may vary with the dryfilm, but we have yet to find a film which does not bond very well to a properly cleaned smooth surface.

  The key issue we find is to clean the copper, dry, and bond the dryfilm immediately, with no hold time between any of the steps.

  I suspect that your dryfilm supplier may be looking for excuses to blame the problems you are having, and they do not really understand the issue.

  Rudy Sedlak
  RD Chemical

Baski Devre  wrote:
  Dear Technetter

To gain best bonding of dry film to the base material some of the
parameters must be controlled strictly such as temperature of rollers of
laminator or sodium carbonate and may be the most critical parameter is
surface roughness. Our dry film supplier suggest roughness value for Rz
1,5 - 3 microns for Ra 0,15 -0 ,3 microns. I want to have your comments
if Rz is normal I mean between 1,5 and 3 microns let us say Rz is 2.10
and Ra is 0.41 microns, how can we interprete or comment on these value;
does it bring good bonding with it or it is an obstacke for dry film to
bond to surface
Thanks in advance for your interpretations and knowledge share
Best Regards

--
Yusuf GÖMEÇ
Product Quality Engineer


BASKI DEVRE SAN ve TIC LTD STI
Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
00 90 216 4836560 (4 Hat/Line)-173(Extention)
Fax: 00 90 216 3544941
00 90 216 4913269
Gsm: 00 90 533 6579897
00 90 533 7480014
msn: [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Sneak preview the  all-new Yahoo.com. It's not radically different. Just radically better.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Sneak preview the  all-new Yahoo.com. It's not radically different. Just radically better.

ATOM RSS1 RSS2