Most of the product in the market is very static generator (
10Kv ). For Kapton tape to be used on PWA look for Antistatic Kapton
Tape.
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Swanson
Sent: Tuesday, June 20, 2006 10:27 AM
To: [log in to unmask]
Subject: Re: [TN] true kapton
My understanding is that it is only the polyimide film which has
anything to do with DuPont (under the "Kapton" trademark). Adhesive tape
manufacturers then put on the adhesive, of which there are a number of
types/chemistries and which is usually proprietary to the tape people.
Actually, my suspicion is that very few if any "Kapton" tapes are made
with DuPont's product any more - there is a shortage, cos the flexi guys
are using it up. See our blog entry:
http://www.intertronics.co.uk/blog/2005/10/eponymous-kapton.html
Normal adhesive types include silicone (for high temperature resistance
- why don't you want it?) and various acrylics.
Regards,
Peter
--
--------------------------------------------------------
Peter Swanson [log in to unmask]
INTERTRONICS http://www.intertronics.co.uk
Tel: +44 1865 842842 Oxfordshire, England
INTERTRONICS is dedicated to providing quality material, consumable and
equipment solutions to the high technology, high performance assembly
industries, incorporating outstanding levels of technical support and
customer service.
Read our blog! http://www.intertronics.co.uk/blog/blog.htm
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: 20 June 2006 15:13
To: [log in to unmask]
Subject: [TN] true kapton
Importance: High
Guys and Gals,
I need help to find real kapton tape with Dupont adhesive... not the
silicone stuff. Any leads are truly appreciated. Thanks in advance.
Best regards,
jk
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|