If the grinding process takes out a "good" joint, you've found the
problem! I like the dye idea, but it still puts the pc board at
risk--and most of the problems I'm trying to solve have to do with
wetting and profile.
Wayne
>>> [log in to unmask] 6/16/2006 2:41 pm >>>
There is a process that uses dye to penetrate the weak or
fractured solder joints. After the dye has a chance to penetrate it is
washed off and the part is snapped off. Any dye left on the pad would
tell you where your fracture/bad solder joint was at, even if the bad
joint was on the BGA side, not on the board side. The problem with
going
the cutting wheel way is that it sounds like you expect the problem to
be at the center of your BGA. By the time you get there, with your
grinder, you would have an opportunity to added enough force and
vibration to cause a failure that my have otherwise not existed.
Ted
---------------------------------------------------------------------------------------
Confidentiality Notice
This e-mail and any attachment(s) are intended for the individual or
entity to which this email is addressed and may contain information that
is confidential. If you are not the intended recipient or an employee
or agent responsible for delivering this e-mail to the intended
recipient, please be aware that any dissemination, distribution or
copying of this communication is strictly prohibited. If you have
received this in error, please notify the sender by telephone at
604.430.4336 or by return e-mail, and please delete or destroy all
copies of this communication. Thank you!
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|