Subject: Re: [TN] Electrical test Failures on Bare Board Finsihes, in
particular OSP
Hi Roland
We have some data and I will try to dig out the relevant files to
send you.
In essence we found that HASL offers the least favorable SIR values
lead or lead-free.
We are presently finishing a major study of lead-free ENIG, ImSn and
ImAg so might have some better info/data-sets by the end of June.
As to your concerns about OSP, from what you describe I would be more
worried about solderability if the OSP is compromised.
Give me a few days to pull out the info...unless you need urgently?
Graham Naisbitt
On 7 Jun 2006, at 16:50, Roland Jaquet wrote:
> Dear Technetters,
>
> Earlier today I sent an email that for some reason got erased. I
> apologize.
>
> I am wondering if there is some knowledge regarding the surface
> electrical
> insulation / resistance depending on the type of Surface Finishes
> such as
> for the bare PCBs as below:
>
> #1 Electroless Nickel Immersion Gold
> #2 Immersion Tin
> #3 HAL Lead free
> Organic Solderability/Surface Preservative
> Electroplated nickel & gold
> Electroless nickel immersion thick gold
> Immersion Silver
> Electroless Nickel & Palladium, Immersion Gold
> Hot air solder leveling
> Electroless Thick Gold
> SAC
> (any finishes I am missing here?)
>
> For instance, I am wondering what could be the resistance of an OSP
> finish
> if the contact is such as a feather and flat, versus conical point
> digging
> in?
>
> Anyone met this kind of problem yet?
>
> In our case, we are considering contact less Electrical Test and we
> worry
> about the different issues we could get in with such a process!
>
> Any suggestion?
>
> Thank you
> Best Regards
> Roland
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16 for additional information, or contact Keach Sasamori
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|