TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Date:
Wed, 7 Jun 2006 09:01:02 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Richard Kraszewski <[log in to unmask]>
Parts/Attachments:
text/plain (165 lines)
See the link

http://www.ipc.org/committeedetail.asp?Committee=5-22G

Rich K / KEDS
260.925.8719
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin D Asbell
Sent: Tuesday, June 06, 2006 2:53 PM
To: [log in to unmask]
Subject: Re: [TN] How are PCB & Assembly manufacturers measuring scrap?

Technical Committee 5-22G??? Which one is this?

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roland Jaquet
Sent: Tuesday, June 06, 2006 12:14 PM
To: [log in to unmask]
Subject: Re: [TN] How are PCB & Assembly manufacturers measuring scrap?

Dear Jack,

Thanks to Denny I learn there is an IPC committee 5-22G in regards to
Production scrap (Rejects) and this subject is of acute interest to me
as I
believe there is some major flows in Bare Board Manufacturing
measurement
of Defect and Rejects.

I do not know how to get information on what has been done and what I
could
read in order to follow the path of the wise men..

I seek to make measurements of Rejects and Defects at the Electrical
Test
level (keeping in mind we are on Bare Boards).

I would appreciate your help as I would appreciate anyone's input as
well.

Thank you very much

PS I am a member of EIPC

Regards to Denny, and thank you.

Meilleures salutations
Very Best Regards
Rol@nd

www.PCBspecialist.com
Roland Jaquet
14 Champ Budin
1258 Perly, GENEVA
Switzerland

Tel         +41-22-880-0405
Fax         +41-22-880-0409
Mobile   +41-79-203-3723

There are three constants in life...
Change, Choice and Principles.
Stephen R. Covey


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz
Sent: Thursday, April 20, 2006 4:18 AM
To: [log in to unmask]
Subject: Re: [TN] How are PCB & Assembly manufacturers measuring scrap?

The assembly side PWB manufacture has worked hard to quanify  yield in
terms
of "defects per million opportunities - DPMO".   While  this is not
actually a
measure of scrap, this does even out differences between  simple and
complex
assemblies

Recently, the same group has started to try to quanify board  fab in
some
similar terms to DPMO.   Board fabrication is not so  easy to quantify
as
it is
harder to define an individual "opportunity".

At Apex/Expo time, this group was collecting the defect codes  from
several
board fabrication shops to try to get a feel for some metrics the
committee
could track.  Anyone interested should contact IPC Committee  5-22G
under
Greg
Hurst of BAE Systems or IPC Technical Staff LIason Jack  Crawford, as a
start.

Denny Fritz
MacDermid, Inc

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2