TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Date:
Mon, 26 Jun 2006 12:44:52 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Stadem, Richard D." <[log in to unmask]>
Parts/Attachments:
text/plain (119 lines)
To an extent, yes. The problem is both the fact that the FR-4 and the
HASL relax. They don't break down, they relax. The immersion silver or
ENIG finish provides a much harder surface to tighten to, and with the
addition of the spring (Bellville) washer the relaxation window is
smaller. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin D Asbell
Sent: Monday, June 26, 2006 12:40 PM
To: [log in to unmask]
Subject: Re: [TN] Plating Recomendation?

I would think, over time, silver and ENIG exposed to atmosphere would
breakdown much sooner than HASL.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, June 26, 2006 12:32 PM
To: [log in to unmask]
Subject: Re: [TN] Plating Recomendation?

Do not use HASL. The reason is that HASL coating is solder, and solder
is soft. Over time, the mechanical connection relaxes as the solder
cold-flows away from under the nuts/bolts/washers. Rather, use a hard
finish such as immersion silver over copper or ENIG. Ideally, the board
pads and the mounting hole rings will all have the same finish, as it is
costly to selectively plate areas of the pwb with a different finish
than is used for the component pads.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Parsons
Sent: Monday, June 26, 2006 12:21 PM
To: [log in to unmask]
Subject: [TN] Plating Recomendation?

Happy Monday!



I have a customer (we are a fabricator) asking the following question;



"..we are looking at making a board that is intended to be bolted to
some batteries through 6mm and 8mm nuts and bolts. I was wondering if
you have any recommendations on what sort of plating should be on the
pads these nuts are going to screw down onto? The batteries are fairly
heavy and the apparatus may be subject to some vibration and shock.
Thanks for your insight."



I am thinking HASL has been used for years in similar applications but
does anyone have any experience or are there any studies on the matter?



Regards



John Parsons




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2