Hi, Badri
You did not specify what type of component or what the lead-free finish
is.
You can usually solder lead-free parts using 63/37 leaded solder without
any problems, if the lead-free finish is matte tin or gold over nickel
or some of the other common finishes. This is true for components with
external leads only, not for BGAs, CSPs, or flipchips with lead-free
balls.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Badri
Sent: Thursday, June 22, 2006 6:22 AM
To: [log in to unmask]
Subject: [TN] lead free compatibility
Hello All,
Can I reflow solder a lead free component (chip components)in the leaded
process/profile. Will there be any solderability issue. Advenace thanks
for the help you are rendering.
Thanx
Badri
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|