Hi,
first it was the cracked capacitor question, thanks to all who answered.
Now I have another one on the ethernal dilemma: is the BGA poorly soldered or there is a design issue?
The question is: how can I assess whether the BGA that fails test is properly soldered? I do not have a 5DX and whatever I can see with the Ersascope looks OK. Needless to say, I cannot get the location of the failed pin.
Will cross sectioning parallel to the surface of the board tell me anything?
Can this be done? Any particularities regarding the polishing of the surfaces?
What to look for?
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------