Ofer
I can assure you that odd layer boards will warp. While you in theory have
the neutral axis coincident with the geometric, in practice there will be
some separation which will cause warp. Since the modulus of elasticity of
the cooper is much greater than that of the prepreg, small changes here
magnify the warp.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Ofer Cohen" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, June 14, 2006 2:16 AM
Subject: [TN] Odd layers count
Hello all,
Due to constraints of PCB thickness and routing dead end I was requested
to approve odd layers count (19 metal layers). I checked the stack up -
it is completely symmetrical, except of the center line that is in metal
layer rather than in laminate or prepreg, as we are used to. Did anyone
experience a problem caused by the non symmetry of laminates versus
prepreg count? Is there availability problem of single-sided laminates?
The material is hi-Tg/hiTd regular FR 4.
Regards
Ofer Cohen
Director - Quality Assurance and Reliability
SIEMENS COM FN A SB
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|