You might have to bond it to reinforce it. Another possibility
is to build up the material around the hole and have it redrilled to
original size.
Ramom
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Lee
Sent: Friday, June 09, 2006 1:57 PM
To: [log in to unmask]
Subject: [TN] Reworking PEM nut on PCBA
Does anyone have recommendation on a process to remove self-clinching
PEM nut from the board? An incorrect 4-40 size and 1/4" long nut was
mistakenly installed and needs to be removed and replaced with a similar
but shorter nut.
Would I lose much of the clinching strength by re-using the hole? Is
there any work-around to reinforce the hole to achieve the similar pull
strength as before?
Any suggestion is appreciated.
Rgds,
Peter
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|