TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jeffrey Bush <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Date:
Mon, 5 Jun 2006 08:53:33 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (143 lines)
The VAC PAC package keeps the boards from abrading and all the bags are
esd/sulfur free. This is good for IT, IS, ENIG or HASL.

Much of this performance also depends on the VAC PAC equipment and
materials that are being used to package with. The variations are large
and this can impact the resulting package.

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
           76 Technology Drive - POB 1890
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 21
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/>
                           

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerald Gagnon
Sent: Saturday, June 03, 2006 11:40 AM
To: [log in to unmask]
Subject: Re: [TN] Packaging requirements for IAg Finished PWBs

Jeffery,

Oops. disagree with you here.... ImAg surfaces must never touch while in
the
package nor should they touch the bag..

I'd be more than willing to pay for this. Can we trade the cost for
leaving
out the useless desiccant?

Gerry


From: Jeffrey Bush <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>, Jeffrey
Bush
<[log in to unmask]>
To: [log in to unmask]
Subject: Re: [TN] Packaging requirements for IAg Finished PWBs
Date: Fri, 2 Jun 2006 11:42:35 -0400

Recommend VAC PAC with not interleaving. Interleaving is and added cost
that is not needed as the boards are held tight in the VAC PAC.

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
            76 Technology Drive - POB 1890
               Brattleboro, Vermont 05302
                 Voice - 802.257.4571 ext 21
                     Fax - 802.257.0011
                        <http://www.vtcircuits.com/>

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gary Camac
Sent: Thursday, June 01, 2006 10:47 AM
To: [log in to unmask]
Subject: [TN] Packaging requirements for IAg Finished PWBs

Good morning all,

I am struggling through a rewrite of our material specification for
PWBs. I
have seen the recommendation that cover sheets and interleaf sheets
should
be used to prevent scratches on IAg finished PWBs. Have those that are
using IAg seen this as necessary? We eliminated this requirement on
Sn/Pb
finished PWBs some time ago without any negative effects.

Thanks,

Gary Camac

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

_________________________________________________________________
Don't just search. Find. Check out the new MSN Search!
http://search.msn.click-url.com/go/onm00200636ave/direct/01/

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2