TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bill Campbell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bill Campbell <[log in to unmask]>
Date:
Wed, 28 Jun 2006 10:04:55 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (136 lines)
probably some buyer decided he could save $.35 on a reel of 5000....

On 6/27/06, Stadem, Richard D. <[log in to unmask]> wrote:
>
> Yes. If they are used for military product, this would ordinarily be
> covered by a GUIDEP alert.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Reuven ROKAH
> Sent: Tuesday, June 27, 2006 8:58 AM
> To: [log in to unmask]
> Subject: Re: [TN] Bad capacitors in Boston Scientific Defibrillators and
> Pacemakers...
>
> There is another important question:
> If it capacitor failure: the capacitor supplier should inform were and
> to whom they were sold and to alert the customers who supposed to use
> them.......
>
> Best Regards
>
> Reuven ROKAH
>
> e mail: [log in to unmask]
>
>
>
> "Tempea, Ioan"
> <itempea@POSITRON
> .QC.CA>
> To
> Sent by: TechNet [log in to unmask]
> <[log in to unmask]>
> cc
>
>
> Subject
> 27/06/2006 16:40 Re: [TN] Bad capacitors in Boston
> Scientific Defibrillators and
> Pacemakers...
> Please respond to
> TechNet E-Mail
> Forum
> <[log in to unmask]>
> ; Please respond
> to
> "Tempea, Ioan"
> <itempea@POSITRON
> .QC.CA>
>
>
>
>
>
>
> I guess there is only one question to be asked: what other sources of
> this kind of products are there?
>
> Ioan
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Stadem, Richard D.
> Sent: Tuesday, June 27, 2006 9:31 AM
> To: [log in to unmask]
> Subject: Re: [TN] Bad capacitors in Boston Scientific Defibrillators and
> Pacemakers...
>
>
> I also found the article disturbing. Some of the facts in the article
> don't quite add up.
>
> They sampled a small percentage. Obviously (I hope) they chose a sample
> size based on the number of defective assemblies they were seeing that
> would ensure the problem caps would be detected if present. I assume
> this was after the fact was discovered. The article states that they did
> not find any bad caps. Was not the sample size large enough, or is the
> problem something else? I am assuming there are capacitors from the bad
> lot still available for inspection.
> All of the bashing of Guidant's processes is not only unprofessional,
> but also very suspicious. These processes are carefully monitored by
> medical quality auditors. If the problem was in product released by
> Guidant and still being manufactured by Boston Sci, how come they did
> not find the problem, either?
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask]
> or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2