TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Kane, Amol (349)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Kane, Amol (349)
Date:
Tue, 27 Jun 2006 11:30:17 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (130 lines)
Hi Bev, 
How was the testing done? Did you use a XRF device? Do you have in place, a sampling plan to test incoming components?
Thanks,

Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing, Inc.
941 Route 38 Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]
www.harvardgrp.com

 -----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Tuesday, June 27, 2006 11:26 AM
To: [log in to unmask]
Subject: Re: [LF] Clarification sought on Pb-containing ceramic

Mike,
Thanks. That's what I thought, but I just wanted some hand-holding. :)


Just for interest for the wider audience, we have caught:
1) A major LCD supplier
2) A major producer of BGAs
3) A major chip manufacturer

Each gave us certified RoHS compliant parts that were not. Now in each
case I am sure that the mistake was not done for devious purposes. In
one case it was an honest misinterpretation of the directive and in the
other two it was an "oops!". Nevertheless, these are cases that could
have come back to bit us. All three involved lead. We have tested
hundreds and hundreds of parts.

Bev
RIM

-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Mike Kirschner
Sent: Tuesday, June 27, 2006 11:13 AM
To: [log in to unmask]
Subject: Re: [LF] Clarification sought on Pb-containing ceramic

Bev,

I've had this discussion with one of the major SMT resistor
manufacturers.
They consider it a glass with a "conductive phase in it"; just the same,
glass or ceramic it's exempt in electronic components.

Mike


On Mon, 26 Jun 2006 08:41:49 -0400, Bev Christian <[log in to unmask]>
wrote:

>"Examples of semimetallic ceramics are lead oxide (PbO), ruthenium
>dioxide (RuO2), bismuth ruthenate (Bi2Ru2O7), and bismuth iridate
>(Bi2Ir2O7). Like metals, these materials have overlapping electron
>energy bands and are therefore excellent electronic conductors. They
are
>used as "inks" for screen printing resistors into thick-film
>microcircuits. Inks are pulverized conductor and glaze particles
>dispersed in suitable organics, which impart the flow properties
>necessary for screen printing. On firing, the organics burn out as the
>glazes fuse. By varying the amount of conductor particles, it is
>possible to produce wide variations in the resistance of thick films."
>Britannica.com
>
>I would presume the use of lead in this instance is exempt. I would
>consider fused lead oxide as a ceramic. That is my interpretation.
>Comments?
>Bev
>RIM
>
>

------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------





CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2