TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Leo Higgins <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Leo Higgins <[log in to unmask]>
Date:
Mon, 26 Jun 2006 22:50:17 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (66 lines)
As Joyce pointed out, Arsenic may be present in very low levels as a grain
refiner in Au. Electroless Ni can be plated with a boron reducing agent
resulting in some boron in the Ni, but this would be unusual for a PCB pad
finish.

Best regards,
Leo

Leo M. Higgins III, Ph.D.
Vice President, Technical Operations
ASAT, Inc.
3755 Capital of Texas Highway, Suite 100
Austin, Texas 78704

office phone 512-383-4593
mobile 512-423-2002
[log in to unmask]
www.asat.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Richard Kraszewski
Sent: Monday, June 26, 2006 9:20 AM
To: [log in to unmask]
Subject: [TN] Boron & Arsenic


Can anyone suggest where in an assembly process I am likely to find
Boron and Arsenic?

I've been presented with an assembly that has some "black crud" on and
around some reflowed SM solder joints. Analysis came back with not only
the "usual suspects" but also these 2 elements. While I am not
eliminating it, for various other reasons I am discounting the
likelihood of the solder paste being the source.

Thanks in advance for your thoughts.

Rich K


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2