TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jeffrey Bush <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Date:
Wed, 14 Jun 2006 08:32:54 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (66 lines)
Generally you can create a balanced construction by using combinations
of core/prepreg. When using a blank layer we will request to repeat the
odd layer to provide symmetry from the center line. If this is not
possible, a single sided core is not used, as you need the venting
pattern/objects in the thief to maintain good resin flow and bonding.

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
           76 Technology Drive - POB 1890
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 21
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/>
                           

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ofer Cohen
Sent: Wednesday, June 14, 2006 2:16 AM
To: [log in to unmask]
Subject: [TN] Odd layers count

Hello all,
Due to constraints of PCB thickness and routing dead end I was requested
to approve odd layers count (19 metal layers). I checked the stack up -
it is completely symmetrical, except of the center line that is in metal
layer rather than in laminate or prepreg, as we are used to. Did anyone
experience a problem caused by the non symmetry of laminates versus
prepreg count? Is there availability problem of single-sided laminates?
The material is hi-Tg/hiTd regular FR 4.

Regards

Ofer Cohen

Director - Quality Assurance and Reliability

SIEMENS COM FN A SB

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2