TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joe Fjelstad <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 2 May 2006 18:57:02 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (31 lines)
In a message dated 5/2/2006 2:23:34 PM Pacific Daylight Time,
[log in to unmask] writes:

Am  looking for a definition of Thieving when applied to PCB  fabs.




Hi Berry,

In some cases it refers to the practice of nasty curs who make  off with gold
scrap and other valuables late at night... ;-)

But I believe that you are asking about non functional areas of the circuit
that are patterned to even out current distribution so that plating is more
uniform, a fairly common practice.

Kind regards,
Joe


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2