Yes. Sometimes I type faster than I read. But I try to help....
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Tuesday, May 23, 2006 10:42 AM
To: [log in to unmask]
Subject: Re: [TN] Connector Shear...
Richard,
Don't worry, you are awake. Steve did send the original email and I
replied to him.
It's rough since we are both Gregory's, but I think Steve is going to
have to change his last name.
Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, May 23, 2006 10:23 AM
To: [log in to unmask]
Subject: Re: [TN] Connector Shear...
Boy am I fast asleep today.
Sorry Jason, I thought Steve sent the email.
And I was wrong about Schleuniger, its Streckfuss.
But I am going so far as to give you the exact part number of the
machine that can do the job. It is CO58, check it out at
http://www.streckfuss.com/co58.htm
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Tuesday, May 23, 2006 10:10 AM
To: [log in to unmask]
Subject: Re: [TN] Connector Shear...
Steve,
Have you considered the Q Corp Lead-o-matic? I've used them in the past
and they work very well (with sharp blades, of course)
http://www.qcorporation.com/lom-ii.html
Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, May 23, 2006 9:54 AM
To: [log in to unmask]
Subject: [TN] Connector Shear...
Morning All!
We have an assembly here that we're trying to reduce the labor on. It's
a rigid-flex board that has this high pin count AbleConn connector
installed.
Take a look at:
http://stevezeva.homestead.com/files/Connector_Top.jpg
and:
http://stevezeva.homestead.com/files/Connector_bottom.jpg
I'm looking for a shear that can trim all the pins to length in one
shot.
You've probably seen them before, you know, a pneumatic foot pedel
operated little gizmo.
I've got a Simonds unit here and am not too happy with it. Besides, it
doesn't have the capability to shear pins in that large of an area.
Fancourt makes a unit called a D-2C/L lead cutter that has a 4" X 4"
working area and should handle this connector. I'm currently waiting on
a quote from them.
I'm just checking with you all to see if you know of anybody else that
might make a lead shear to do this connector. There's over 450 pins on
this little jewel and we're having to trim them one-by-one.
I know what you're thinking and before you ask, I already checked. We
can't get the connector with the pins already trimmed to the length we
need them...
Kind regards,
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|