Hello Technetters,
I need your help on the following thermal cycle test problem.
Recently we asked our PCB suppliers to do 1000 cycle thermal cycle test for 6L, daisy chain boards with plated through holes filled with epoxy ink and cap plated on the top of the holes( or via-in-pad design). The resistance change before and after thermal cycle test is less than 5%, however the holes have complete barrel crack. Have you seen this kind of problem before? Can I approve the supplier's test result?
Here are some more information about the test for your reference.
1) board thickness: 1mm (40mils)
2) hole size: 20mils, 18mils, 15mils, 10mils. All have complet barrel crack except the holes of 10mils .
Thanks for your help in advance!
Chris
__________________________________________________
¸Ï¿ì×¢²áÑÅ»¢³¬´óÈÝÁ¿Ãâ·ÑÓÊÏä?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
http://cn.mail.yahoo.com