Bromine as a flame retardant in laminate isn't banned under Rohs or
leadfree, therefore FR4 is ok.
Colin McVean M.Inst.C.T.
Production Manager
Artetch Circuits Limited
Main: 01903 725365
DD: 01903 712926
Email: [log in to unmask]
www.artetch.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Ball
Sent: 17 May 2006 15:26
To: [log in to unmask]
Subject: [TN] Rohs Weeeeeee board material
Hello Folks-
We're trying to cost a new design which may have to be leadfree, rohs
compliant, etc...
We would otherwise reference IPC4101/21. Any recommendations as to what
we
should specify for this one? We were gonna ref. /24 but that's got
bromine......
Thanks in Advance,
-Chris
"This e-mail message is intended only for the use of the intended
recipient(s).
The information contained therein may be confidential or privileged, and
its disclosure or reproduction is strictly prohibited.
If you are not the intended recipient, please return it immediately to
its
sender at the above address and destroy it."
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|