Right. There is no a perfectly good board finish. Everyone has its own pros and cons. With Pb-free it's getting even more complicated. We have to know which failure mode we might face for a given finish and I believe that "Black Pad" is not the most dangerous one anymore.
Regards,
Vladimir
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee parker
Sent: May 15, 2006 10:00 AM
To: [log in to unmask]
Subject: Re: [TN] Question about ENIG in SnPb process . . . .
Sefika
There are a number of flat metal finishes from which to choose: immersion
silver, flash gold etc. These generally perform well; however, when a
process goes out of the processing limits you can expect trouble. It is the
suppliers job to insure this does not occur or that all questionable product
is captured. It is the OEM's job to set the end point specs.
Regardless of the finish you select, I suggest you go through a
qualification process and then place end point requirements on the product
and that you rigorously enforce these requirements. I know of one OEM that
has a very long check list of end point requirements that are enforced.
Although it was inconvenient and expensive to the supplier, great care is
taken with their product. This OEM seldom has quality issues once the
supplier understands the consequences.
Best regards
Lee
----- Original Message -----
From: "Şefika ÖZKAL" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, May 15, 2006 2:19 AM
Subject: Re: [TN] Question about ENIG in SnPb process . . . .
> Dear Technetters,
>
> Instead of ENIG what should we choose? For example, for high density (with
> bgas) boards with some of the components lead-free plated?
>
> Moreover what is the choice when the components assembled to the boards
> are
> both lead-free alloy plated and lead alloy plated (mixed)?
>
> Regards
>
> Sefika
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
> Sent: Friday, May 12, 2006 11:52 PM
> To: [log in to unmask]
> Subject: Re: [TN] Question about ENIG in SnPb process . . . .
>
> LOL Werner,
> I totally understand where you are coming from. As a process engineer,
> you should see how much hell I need to go through to verify that the
> root cause of the solder reliability issues is not the process but the
> pwb finish, or issues related to it. And identifying surface finish
> problems is not easy, nor cheap. We usually need to go to an outside
> failure analysis house to get verification. This is very costly. Thus I
> also have a somewhat biased opinion towards ENIG using standard 63/37
> solder. And as you pointed out, Werner, the lead-free alloys combined
> with ENIG makes the situation potentially much worse.
> With ENIG, some of the plating issues are exacerbated by further thermal
> cycles during normal processing. This is why it is difficult to prove
> "is it the plating, or is it the process". There quite often are
> situations where it is a little of both.
> When I am working with military hardware (or really, any electronic
> assemblies), the last thing I want to take a chance on is solder
> reliability issues with the board finish that go undetected until
> hundreds or even thousands of assemblies are built and in the field.
> Because of ENIG's fickle nature, and because I do not like to solder to
> nickel for all of the reasons that are well documented here in the forum
> archives and hundreds of white papers, articles, and so forth, I simply
> try to stay away from it whenever possible. Why would I ever need to use
> it, except for in certain situations and space applications where it is
> not qualified?
>
> And Gerard, I want you to understand I respect your knowledge and
> opinions fully, I simply choose to disagree with you on this.
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
> Sent: Friday, May 12, 2006 1:15 PM
> To: [log in to unmask]
> Subject: Re: [TN] Question about ENIG in SnPb process . . . .
>
> Thanks Lee, Richard & Daniel,for backing up my experience.
>
> Gerard, of course, as a consultant clients come to you when they have
> problems, not when everything works as advertised. So, purely
> statistically, consultants get a one-sided picture.
> As a consultant, one of your first obligations is to do no harm with our
> advice [sort of like physicians]-having seen what I have, there is no
> way I can advise a client in favor of ENIG. Of course it works most of
> the time, but God help me i advice ENIG to a client and all hell breaks
> loose.
>
> Werner
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
>
>
> Dikkat :
> Bu elektronik posta mesajı kişiseldir. Eğer, gönderilmesi
> gereken kişi değilseniz lütfen göndericiyi bilgilendirip
> mesajı siliniz. Firmamıza gelen ve giden mesajlar virüs
> taramasından geçirilmekte, hukuki nedenlerle log kayıtları
> tutulmaktadır. Mesajdaki görüşler ve bakış açısı göndericiye
> ait olup Aselsan A.Ş. resmi görüşü olmak zorunda değildir.
>
> Attention :
> This e-mail message is private.
> If you are not the intended recipient please delete
> the message and notify the sender. E-mails to and
> from the company are, monitored for virus protection
> and in accordance with lawful business practices.
> Any views or opinions presented are solely those of the
> author and do not necessarily represent the views of
> Aselsan A.S.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|