Usually, resistance is monitored continuously during these tests and the
important information is the number of cycles before failure. Was this
an Interconnect Stress Test arrangement, where the vias are heated by
passing a current through them? I'm guessing not, since it was a daisy
chain and they all failed, whereas in the IST it would stop on or before
the first failure.
What was the temperature range for the thermal cycle test? In order
for the boards to pass despite barrel cracks/breaks you would have to
make the case that the temperature range used was way too high for your
application. So either the boards are bad or the test was useless.
Wayne Thayer
>>> [log in to unmask] 5/23/2006 2:52:57 am >>>
Hello Technetters,
I need your help on the following thermal cycle test problem.
Recently we asked our PCB suppliers to do 1000 cycle thermal cycle
test for 6L, daisy chain boards with plated through holes filled with
epoxy ink and cap plated on the top of the holes( or via-in-pad design).
The resistance change before and after thermal cycle test is less than
5%, however the holes have complete barrel crack. Have you seen this
kind of problem before? Can I approve the supplier's test result?
Here are some more information about the test for your reference.
1) board thickness: 1mm (40mils)
2) hole size: 20mils, 18mils, 15mils, 10mils. All have complet
barrel crack except the holes of 10mils .
Thanks for your help in advance!
Chris
__________________________________________________
?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
http://cn.mail.yahoo.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|