TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Mikell <[log in to unmask]>
Date:
Fri, 19 May 2006 09:34:04 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
From:
John Burke <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (130 lines)
Sunshine and a beer Steve?

I will be pushing the bike around bends on highway 9 this weekend out
towards Santa Cruz...................8-)

Have a great weekend all.........

John

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Mikell
Sent: Friday, May 19, 2006 1:14 AM
To: [log in to unmask]
Subject: [TN] [NTC]Re: [TN] Tin Whisker REVENGE

Phil,

we're talking about justice here. nobody but the lawyers see any money
(aren't judges lawyers too, wonder how they get their share?).

The idea here would be...
1. Correct a grave injustice against humanity
2. Screw the turkeys who ignored their own written procedures to pass a law
to gain some kind of brownie points.
  (question.. what ISO spec must governments operate under and be certified
to????)

some things to think about....
critical systems that involved public safety were to be exempt.... isn't
the EU adopting an enhanced 911 type system called E112..  see link
http://wireless.iop.org/articles/news/5/12/4/1
So cell phones with e112 features should be considered exempt????

also... is it possible that regarding RoHS and WEEE have the EU has ulterior
motives which are not spoken of?

As an example of ulterior motives, I offer a cautionary tale from my
youth.....
The year, 1980. Location: USA, California's San Fernando Valley
Company: the world's largest independent manufacturer of computer printers.
They decided to transfer all PCA production to a division in Hong Kong,
claiming via an internal memo, that it would save an average of 40USD per
unit. My boss
decided I should do an in depth analysis, which resulted in my publishing a
white paper that showed about 4USD per unit loss plus substantial
intangibles that made this a bad decision. shortly after publishing the
paper, i was told to turn over all work product and copies related to this
project, and be a good boy and shut-up. Seems the real reason was for tax
accounting reasons, and to avoid paying taxes by shuffling money out of the
US (and 50% taxes) to Hong Kong (17%, as I recall). Seems the internal memo
was a cover for the IRS if they ever looked into this.

While the original ideas behind WEEE and RoHS may have been legit, Europe
has been struggling with cheap labor more than the USA for years, and these
laws may have become an attempt to erect trade barriers. If nothing else,
these laws have provided support to capital equipment manufacturers
supplying new Pb-free machines. I have seen few consultants or trade groups
or other organizations speak against WEEE/RoHS because it has been a
windfall of work, grants, membership, workshops, etc... so they aren't going
to sling arrows at their golden goose.  Some heavyweights like Werner do
speak, but they are few.

I don't have an IPC membership list, so when IPC claims it took its passive,
"fait accompli"? approach as being the will of its membership, I don't know
what that really meant.  I did pull the membership list from iNEMI, and
found the following:
Institutes of education                     4
EMS companies                               5
OEMs                                       20
Agencies                                    7
Green companies                             8
(companies who help you be green)
Suppliers to the industry                  34
To my way of thinking, only the OEMs want RoHS stopped, but are afraid of
backlash. That would make the vote on RoHS 58 for and 20 against. The
non-OEMS would be pro-RoHS, because EDUs, EMSs, Agencies, greenies and
suppliers can look at RoHS as a financial opportunity, a chance to raise
prices, sell new products, break down barriers to sales, get new funding,
increase margins....

The OEMs need an IPC to be their front guy, to shield them from direct
attack. The IPC, as a technical group, can shout out that the EUs Emporer
has no clothes on..., but they wimped out.. (hey, but thanks for letting us
use your forums!!)

But now we have the Great and All Powerful Burke... Long live the Burke...

Yes, that felt good... gotta get some sunshine this weekend, and a beer

Steve Mikell

> Phil Nutting wrote
> And will the lawsuit reimburse all the companies for what they have
> invested in this misguided change?
>
> Just my personal opinion.
>
> Phil
>
>


--
___________________________________________________
Play 100s of games for FREE! http://games.mail.com/

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2