Bromine is NOT disallowed, only a couple of specific bromine compounds
that are not normally found in laminates. Most FR4 is flameproofed by
tetrabromobisphenol A which is permitted.
Brian
Chris Ball wrote:
> Hello Folks-
>
> We're trying to cost a new design which may have to be leadfree, rohs
> compliant, etc...
>
> We would otherwise reference IPC4101/21. Any recommendations as to what we
> should specify for this one? We were gonna ref. /24 but that's got
> bromine......
>
> Thanks in Advance,
> -Chris
>
>
>
> "This e-mail message is intended only for the use of the intended
> recipient(s).
> The information contained therein may be confidential or privileged, and
> its disclosure or reproduction is strictly prohibited.
> If you are not the intended recipient, please return it immediately to its
> sender at the above address and destroy it."
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
--
http://www.cypenv.org Cyprus environment/energy
http://www.cypenv.org/worldenv World environment/energy
http://www.cypenv.org/weather Cyprus weather
http://www.cypenv.org/smf/index.php Environment/energy forums
http://groups.yahoo.com/group/cypnature/ Cyprus nature forum
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|