TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, David Tremmel <[log in to unmask]>
Date:
Mon, 8 May 2006 11:46:45 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (85 lines)
        Good article David:
http://www.speedlinetechnologies.com/docs/Frank-Grano_SMTA2004.pdf
        Regards,
        Ramon
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Tremmel
Sent: Monday, May 08, 2006 10:16 AM
To: [log in to unmask]
Subject: Re: [TN] Intrusive Reflow

Hello,

Would anyone care to define what an intrusive reflow is?

TIA,

David

>From: Yannick Brisson <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>,              Yannick
>Brisson <[log in to unmask]>
>To: [log in to unmask]
>Subject: [TN] Intrusive Reflow
>Date: Mon, 8 May 2006 09:04:05 -0400
>
>Hi,
>
>         Does anyone have tried intrusive reflow with any king of lead 
>free material??  I'd like to have your input on that topic.  I'm 
>wondering if the sames rules applied to SnPb and Lead Free? Do you know

>if it is better with a Tin , Silver or Gold plating? Do we need to have

>more paste applied to the board to met the IPC standard?
>
>Thank you
>
>Yannick
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To 
>unsubscribe, send a message to [log in to unmask] with following text in 
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
>or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing 
>per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: 
>http://listserv.ipc.org/archives Please visit IPC web site 
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask]

>or 847-615-7100 ext.2815
>-----------------------------------------------------

_________________________________________________________________
MSN Latino: el sitio MSN para los hispanos en EE.UU.
http://latino.msn.com/

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2