Barry: In regards to plating.
Thieving: Features placed on the outerlayer of the board to balance the
plateable surface area, producing uniform current distribution during
electroplating. Thus providing a consistent plating thickness across the
board and in the holes.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Barry Gallegos
Sent: Tuesday, May 02, 2006 2:22 PM
To: [log in to unmask]
Subject: [TN] Thieving
Good day T'Netters.
Am looking for a definition of Thieving when applied to PCB fabs.
Thank you in advance
Barry
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
This message (including any attachments) contains confidential and/or
proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on the
contents of this information is strictly prohibited and may constitute a
violation of law. If you are not the intended recipient, please notify
the sender immediately by responding to this e-mail, and delete the
message from your system. If you have any questions about this e-mail
please notify the sender immediately.
Ce message (ainsi que les 'eventuelles pi`eces jointes) est
exclusivement adress'e au destinataire et contient des informations
confidentielles. La copie, la communication ou la distribution du
contenu de ce message sans l'accord pr'ealable de l'exp'editeur sont
strictement interdites et peuvent constituer un d'elit. Si vous n'^etes
pas le destinataire de ce message, merci de le d'etruire et d'avertir
l'exp'editeur. Si vous avez des questions se rapportant `a ce courrier
'electronique, merci de bien vouloir notifier l'exp'editeur
imm'ediatement.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|