Hi Lee,
Forgive my ignorance, but could you please explain what you mean by the
statement "silver inventory is increased many times over"? Are you meaning
that the deposition thickness of electrolytic silver is higher than that
found for immersion silver thereby allowing for an increased risk of metal
migration?
Best regards,
Joe Russeau
----- Original Message -----
From: "Lee Parker" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, May 24, 2006 3:21 PM
Subject: Re: [TN] Electrolytic Ag Suppliers for COB applications
> Steven
>
> I would be careful about electrolytic silver in electronic applications.
> While this has not been a problem with immersion silver there have been
> problems with silver migration using electrolytic silver. Most likely,
> because the silver inventory is increase many times over.
>
> Best regards
>
> Lee
>
> J. L. Parker Ph.D.
> JLP Consultants LLC
> (804) 779 3389
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Creswick, Steven
> Sent: Wednesday, May 24, 2006 3:00 PM
> To: [log in to unmask]
> Subject: [TN] Electrolytic Ag Suppliers for COB applications
>
> All,
>
> I do not wish to get any plating bath suppliers in trouble by responding
> to the forum at large [and come across as selling themselves], but if
> there is anyone lurking out there in the bushes that knows of a plating
> bath supplier selling electrolytic Ag for gold wire bonding
> applications, please contact me directly. I am speaking of automotive
> type quantities, but can not really get into the application.
>
> The underlying nickel could be electroless or electrolytic.
>
> Would like US and overseas users of said bath/s if possible.
>
> Have checked the archives, but did not locate appropriate info
>
>
> Steven Creswick
> Gentex Corporation
> 616 772 1590 x846
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|