TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 3 May 2006 07:30:00 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Steve Gregory <[log in to unmask]>
Parts/Attachments:
text/plain (134 lines)
Au contraire! I'll help you. There are four Dairy Queens in the
immeadiate Dallas area. Click on, or copy and paste the whole link below
into your browser. No excuses now man...hehehe. 

 
http://www.dairyqueen.com/en-us/locate%20a%20store/MapQuestSearchResults
.htm?&city=Dallas&stateProvince=TX&country=US&clientId=30235&imageType=p
ng&maxSearchResults=10&pheight=365&proxIconId=400&pwidth=365&radius=100&
search1=1&searchQuantifier=AND&srchIconId=400&transaction=search&units=m
i

-Steve Gregory-

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Wednesday, May 03, 2006 7:05 AM
To: [log in to unmask]
Subject: Re: [TN] Surface Tension Data for SAC305

Yah, like Dave's gonna be able to find, and deliver, a Dairy Queen ice
cream cone, in Dallas, in September.  Sucker bet........

Doug Pauls




             "Gregg A. Owens"
             <Owensmttc@EARTHL
             INK.NET>
To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>
cc

 
Subject
             05/02/2006 06:36          Re: [TN] Surface Tension Data for
             PM                        SAC305


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
             "Gregg A. Owens"
             <Owensmttc@EARTHL
                 INK.NET>






Dave:

Like the way you bribe folks for technical information.

Gregg A. Owens, MIT
Manufacturing Technology Training Center, Inc.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, May 02, 2006 8:33 AM
To: [log in to unmask]
Subject: [TN] Surface Tension Data for SAC305

Hi TechNet land! Hey, need some speedy assistance - the JSTD-002 and
JSTD-003 committees need a piece of technical data. We are looking for
the surface tension of SAC305, in J/m2, at 255C. Anyone who can supply
that value will win a large chocolate ice cream cone from Dairy Queen
courtesy of me at the next IPC meeting!

TIA!

Dave Hillman
JSTD-002/003 Chairman
[log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2