Hi Gregg! Such an innocent question which lands you in such a huge
minefield! The best summary one can give is "it depends" (cha-ching, Doug
gets another Mt. Dew). Many, many component finish, flux chemistry and
reflow profile detail interactions to understand and deal with. I recommend
that your student attend one of the tutorial or workshops that are part of
either the IPC or SMTAI conferences and/or look at some of the large
consortia reports (INEMI, CALCE, UIC, JCAA/JGPP, NIST, NPL, etc.) to get a
better understanding of a large complex issue. Soldering Pbfree finished
components in a SnPb process is very achievable provided a person has
completed their homework.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Gregg A. Owens"
<Owensmttc@EARTHL
INK.NET> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
05/02/2006 12:26 [TN] Mixing Lead-free Plated Parts
PM with Leaded Solder
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
"Gregg A. Owens"
<Owensmttc@EARTHL
INK.NET>
Dear Technetters:
One of my students have asked a good question. Can one take lead-free
plated
parts (likely Sn100) and solder using Sn63 without any significant
metallurgical concerns? I believe this issue was previously discussed but
can't find it in the archives.
Your thoughts appreciated.
Gregg Owens, MIT
Manufacturing Technology Training Center, Inc.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|