TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 17 May 2006 10:18:37 +0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Lum Wee Mei <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (27 lines)
Hello,

I flipped through the whole of IPC 620 but did not find anything about insertion
pin height. I remember in the old MIL std, it mentioned that inserted pin must
ensure to have level height to consider acceptable. Is this criteria no longer
important?

The reason I asked is because we come across some connectors have their inserted
pins being pulled back into the socket after the wires are tighten. Should it
not consider reject? If such connectors with sunken pins are plugged into their
mating part, the connectivity will be a problem

For your kind advice.

Thanks and regards,
Wee Mei

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2