I would be of the opinion that the Cu-Sn intermetallic growth is more dependent on the temperature than time. If processed and stored correctly, the boards can last well over 6 months.......
Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing
941 Route 38 Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of George Carroll
Sent: Friday, April 28, 2006 9:29 AM
To: [log in to unmask]
Subject: Re: [TN] Shelf life of circuit board plating
I have had ENIG boards from a reputable supplier that have soldered well long after 6 months. As you questioned, moisture absorption of the substrate, if left open, could lead to other problems depending on normal local R.H. With regard to ImSn, sealed or not, your're going to see solderability problems at 6 months or before from Cu-Sn intermetallics. As discussed here and elsewhere, a Ni barrier layer over the copper could mitigate that but I'm not sure how widely available it is or what new problems it might create.
George
State of Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Phil Nutting
Sent: Friday, April 28, 2006 9:03 AM
To: [log in to unmask]
Subject: [TN] Shelf life of circuit board plating
Good Friday Morning All,
This topic may have been previously discussed, but let me try to phrase
my "problem" completely so the answer can be simpler.
I have a board vendor (Fab house) stating that for my ENIG boards the
plating only has a 6 month shelf life if the package is opened. Did I
miss something here? I thought Gold doesn't tarnish.
If this is true, then Immersion Tin, Immersion Silver and ENIG all have
storage issues.
OK, so I open a sealed package and take out half of the boards in the
package. I may not need the rest of the boards for many months. So how
do I protect the unused boards? Should I vacuum seal them? Add a
desiccant? If I add a desiccant, are there different desiccants which
might damage the boards?
I'm sure I'll have more questions right after I send this.
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|