When I read this, before all the other replies, I said to myself,
"Whoa!, this is REALLY nasty stuff!" The EU labelling classification is
Symbol: F, Xi, T
R: 11-19-36/37
S: (2-)-16-28-29-33
Highly flammable
Irritant
Toxic
May form explosive peroxides
Irritating to eyes and respiratory system
Keep out of the reach of children
Keep away from sources of ignition - No smoking
After contact with skin, wash immediately with plenty of water
Do not empty into drains
Take precautionary measures against static discharges
However, that's not all. How does it work? It doesn't chemically react
with the paraxylylene of the coating, but it penetrates into the polymer
matrix, causing it to swell and thus destroy the bonding to the
substrate. As it is volatile, so the vapour will do the same, to a
lesser extent, with surrounding coating and this may well destroy the
integrity of the bond sufficiently for the reliability to be affected,
even if you cannot see the damage.
My advice: don't! The laser method is inherently better and cost should
not be a criterion.
Brian
Steve Gregory wrote:
> Hi All!
>
> I've always thought that when it comes to removing parylene coating,
> about the only way you can remove it is with some sort of mechanical
> means, i.e.; microabrasion, or scraping. Burning through it with a
> soldering iron when trying to do rework it is very, very
> difficult...I've tried it...it doesn't work well at all.
>
> I was just told that a chemical that I haven't heard of before might
> work, it's called THF, or Tetrahydrofuran. I was told that it won't
> dissolve the coating, but will cause it to lift from the PCB where it
> can be brushed away. Have any of you ever heard of this stuff? I'm not a
> chemist, and I'm not about to use it until I learn more about it.
>
> The issue that I have is with a little tiny assembly that has been built
> and parylene coated with some bad programmable hall effect switches
> installed. The board is so small, and there are other components
> installed really close to where the coating has to be removed. I'm
> afraid of getting them microblasted because I'm afraid of damaging the
> other components. See the assembly at:
> http://stevezeva.homestead.com/files/8001_assy_backside.JPG ...the small
> components are 0402's, so that gives you a visual scale of how big the
> assembly is...
>
> I've got the information in to a company that I found that does laser
> ablation to remove coatings to give us a quote, so I'm waiting on that.
> But if that turns out to be really expensive, I was contemplating using
> the THF as plan "B" (provided the stuff will work and it doesn't hurt
> anything else on the assembly).
>
> Kind regards,
>
> -Steve Gregory-
> Senior Production Engineer
> OAI Electronics
> East 12th Street
> Tulsa, Oklahoma 74112
>
> (918) 836-9077 Ext.-507
> (918) 706-2779 CELL
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
--
http://www.cypenv.org Cyprus environment/energy
http://www.cypenv.org/worldenv World environment/energy
http://www.cypenv.org/weather Cyprus weather
http://www.cypenv.org/smf/index.php Environment/energy forums
http://groups.yahoo.com/group/cypnature/ Cyprus nature forum
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|