Hi all,
I have come across papers that authoratively state both! Some say that newer Immersion Sn finish have additives that mitigate the growth of whiskers, while some say that Immersion Sn is still prone to whisker growth and that every surface with Immersion Sn should be soldered to, to prevent whiskers. Its still one of those classical quandaries. I think the best way (not the most feasible) is to perform Sn whisker testing on individual Immersion Sn surface finish before actual use (again, not feasible!) so that the vendor Immersion Sn process can be qualified.
Any thoughts/additions? BTW we have used Immersion Sn and Immersion Ag finishes with success in our lead-free transition
Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing
941 Route 38 Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden
Sent: Friday, March 24, 2006 12:16 PM
To: [log in to unmask]
Subject: Re: [TN] Tin Whisker Mitigation
I believe immersion tin DOES promote whiskers, although not at the same
level as electrolytic tin. Check IPC-4554, especially Appendix 6. "A
potentially significant source for whisker formation are stresses induced
from formation of CuSn IMCs....Whiskers have grown on immersion tin
conductive features. To date, these whiskers have appeared at ambient
conditions..."
As for using cc for mitigation, it has also been found that whiskers will
still grow under (and even penetrate) coating. Check NASA paper "Effects of
Conformal Coat on Tin Whisker Growth".
Regards,
Kevin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Friday, March 24, 2006 11:34 AM
To: [log in to unmask]
Subject: Re: [TN] Tin Whisker Mitigation
Dewey:
I hear you loud and clear. In the near future thanks to some
crazy fellows that want to save the earth.... We may have to go that route
per customer request. Other choices ensure that the Tin finish is Matte,
bigger grain, instead of bright tin ( do not know yet how to verify that),
have at least 3% Pb or 3-5% Bi( use of XRF) , CC assembly, annealing
components, reflow assembly, immersion Tin finish.... My understanding of
Immersion tin is that it does not promote Whiskers. The problem that I know
about this finish, ImSn, is that it is too thin and IMC form to make it
unwetable.
Thanks for your sharing,
Regards,
Ramon
-----Original Message-----
From: Whittaker, Dewey (AZ75) [mailto:[log in to unmask]]
Sent: Friday, March 24, 2006 10:39 AM
To: TechNet E-Mail Forum; Dehoyos, Ramon
Subject: RE: [TN] Tin Whisker Mitigation
Ramon,
Yes.
Don't do it and spare yourself the cruel and unusual punishment.
Depending on your customers and critical end-use applications, the amount of
effort to do this and control it is incredible. It can be done, but it
extracts a heavy toll. Even meager efforts in-house with chips is a waste of
dough( now class did you catch the joke? Toll house morsels = Chips(
chocolate) = waste of dough. Good you earned your chocolate chip cookie).
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Friday, March 24, 2006 8:18 AM
To: [log in to unmask]
Subject: [TN] Tin Whisker Mitigation
Hello TechNetters:
Does anyone know of companies that are replating parts with Sn63
and reballing BGAs? Could any one share their experiences in
doing this effort? Things such as: extra time needed, cost,
reliability.......
Regards and TIA,
Ramon Dehoyos,
410.552.2210
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|