The original specification MIL-P-13949 has class 1, 2, 3 and 5 for basic FR4. The IPC-4101 has classes A, B, C and D following the same basic tolerances for thickness - A=1, B=2, C=3 and D=5 - so using class B IPC-4101 for Class 2 products makes sense. Laminate suppliers and PCB houses will have no issues meeting these tolerances and I would use the B thickness tolerance for both Class 2 and Class 3 end-product requirements as these are inline with inherent capability of both materials and PCB fabrication.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice - 802.257.4571 ext 21
Fax - 802.257.0011
<http://www.vtcircuits.com/>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of "Sefika ÖZKAL"
Sent: Friday, April 14, 2006 9:03 AM
To: [log in to unmask]
Subject: Re: [TN] laminate thicknesses
Hi Jeffry,
Thank you for your answers.
Is only Class B is compatible with class 2 or may I conclude that if Class B
is Ok,then C is also?
Regards
Sefika OZKAL
-----Original Message-----
From: Jeffrey Bush [mailto:[log in to unmask]]
Sent: Friday, April 14, 2006 3:48 PM
To: TechNet E-Mail Forum; Şefika ÖZKAL
Subject: RE: [TN] laminate thicknesses
Class B is compatible with class 2.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice - 802.257.4571 ext 21
Fax - 802.257.0011
<http://www.vtcircuits.com/>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of "Sefika ÖZKAL"
Sent: Friday, April 14, 2006 6:55 AM
To: [log in to unmask]
Subject: [TN] laminate thicknesses
Hi Technetters,
According to IPC4101, there are Class A , B, C and D laminates. Which of the
laminates are prefered if the PCB specification is IPC6012-Class II?
I have looked up IPC4101, but I could not find any thing?
Do you have an idea?
Thanks,
Sefika OZKAL
Design Engineer
ASELSAN INC. MGEO Division
Address : Cankiri Yolu 7. Km
Akyurt Ankara TURKEY
E-mail : [log in to unmask]
Tel : +90 312 84 75 300 Ext: 4698
Fax : +90 312 84 75 320
Dikkat :
Bu elektronik posta mesajı kişiseldir. Eğer, gönderilmesi
gereken kişi değilseniz lütfen göndericiyi bilgilendirip
mesajı siliniz. Firmamıza gelen ve giden mesajlar virüs
taramasından geçirilmekte, hukuki nedenlerle log kayıtları
tutulmaktadır. Mesajdaki görüşler ve bakış açısı göndericiye
ait olup Aselsan A.Ş. resmi görüşü olmak zorunda değildir.
Attention :
This e-mail message is private.
If you are not the intended recipient please delete
the message and notify the sender. E-mails to and
from the company are, monitored for virus protection
and in accordance with lawful business practices.
Any views or opinions presented are solely those of the
author and do not necessarily represent the views of
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Aselsan A.S.
Dikkat :
Bu elektronik posta mesajı kişiseldir. Eğer, gönderilmesi
gereken kişi değilseniz lütfen göndericiyi bilgilendirip
mesajı siliniz. Firmamıza gelen ve giden mesajlar virüs
taramasından geçirilmekte, hukuki nedenlerle log kayıtları
tutulmaktadır. Mesajdaki görüşler ve bakış açısı göndericiye
ait olup Aselsan A.Ş. resmi görüşü olmak zorunda değildir.
Attention :
This e-mail message is private.
If you are not the intended recipient please delete
the message and notify the sender. E-mails to and
from the company are, monitored for virus protection
and in accordance with lawful business practices.
Any views or opinions presented are solely those of the
author and do not necessarily represent the views of
Aselsan A.S.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|