TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 11 Apr 2006 18:12:00 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (93 lines)
Hi Steve - Rockwell Collins has 5 Vapor Phase systems and they are a very
good tool to have in the soldering tool box. There are three ways to melt
solder: conduction (a soldering iron, wave soldering), convection (a reflow
oven, a hot air rework station) and condensation (a vapor phase system).
Sometimes condensation soldering is the perfect tool. We use both 3M and
Galden fluids. You should be able to solder both SnPb and Pbfree with a
230C Vapor Phase fluid. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




             Steve Gregory
             <SGregory@OAIELEC
             TRONICS.COM>                                               To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             04/11/2006 10:32          [TN] RD Technologies Vapor Phase
             AM                        Users


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
               Steve Gregory
             <SGregory@OAIELEC
               TRONICS.COM>






Mornin' All!

I've just got the opportunity to work with a new vapor phase reflow
system here at my new position. It's a RD Technologies RD3 with a vapor
recovery system. We're in the process of hooking it up, we haven't yet
started it up.

I worked with a vapor phase many years ago (1988), and this system is
much nicer than what I remember about the system I worked with in the
past.

I was wondering if there are any RD Technologies users out there that
have any "words of wisdom" that they might share with me about the
system I'm that going to be working with. BTW, we're going to using
Galden heat transfer fluids.

Kind regards,

-Steve Gregory-
Senior Production Engineer
OAI Electronics
6960 East 12th Street
Tulsa, Oklahoma 74112

(918) 836-0507
(918) 706-2779 CELL
(918) 836-0184 FAX

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2