TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Todd, Richard" <[log in to unmask]>
Date:
Wed, 26 Apr 2006 09:36:43 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Schaefer, Chris" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Schaefer, Chris" <[log in to unmask]>
Parts/Attachments:
text/plain (98 lines)
Well guys I will start using this product (MS2100PB - PKay Metal) within the next couple of weeks. I will be using the leaded version of the surfactant to start off with until I feel that has no detriment to my process and performs adequately well to continue its use.

I will let you all know of my results.

Chris Schaefer
Suntron Corporation
Process Engineer
540 N. Rogers Road
Olathe, Kansas 66062
913.393.5878
[log in to unmask] 

NOTICE:
 
This message is intended for the use of the individual entity to which it is addressed and may contain information that is privileged, confidential and exempt from disclosure under applicable law. If the reader of this message is not the intended recipient, or the employee or agent responsible for delivering the message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by calling 913.393.5878 or returning the original message to us.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Todd, Richard
Sent: Wednesday, April 26, 2006 8:48 AM
To: [log in to unmask]
Subject: [TN] Molten Solder Surfactant for Dross Elimination


TechNet,



I have come to the Oracle seeking wisdom.  Has anyone had any experience
with using a molten solder surfactant for dross elimination in a wave solder
process?  There is a (fairly) new product on the market which makes some
exciting claims.  Although, as the adage goes, if it sounds too good to be
true, it probably is!

I am not a chemist or metallurgist but, I think I understand in principal
how this stuff works, but I am hesitant to add anything to my solder pot for
fear of contamination issues, etc.  Any and all comments are welcome.  I am
especially concerned about long-term solder joint reliability issues.  I
will do my own testing and validation both in lab and on the production
floor but I want to understand any process concerns, etc.



Oh, by the by, I am running standard Sn/Pb in my waves; we do not solder in
an inert environment and we do not clean our boards (no-clean flux).



Thanks in advance,



Rick Todd

Senior Engineer

Process Quality Engineering



Panasonic Automotive Systems Company of America

Division of Panasonic Corporation of North America

776 Highway 74 South, Peachtree City, GA 30269

770-515-1087 Direct

678-458-2887 Cell

770-486-2248 Fax

[log in to unmask] <mailto:[log in to unmask]>




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2