TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Thu, 20 Apr 2006 15:05:48 -0700
Reply-To:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
Subject:
From:
Ahne Oosterhof <[log in to unmask]>
X-cc:
Chris Block <[log in to unmask]>
In-Reply-To:
Organization:
A-Laser, Inc.
MIME-Version:
1.0
Parts/Attachments:
text/plain (86 lines)
A very nice (but not cheap) method is laser ablation. I have done this to
remove soldermask off some pads on a very expensive board with very
expensive components and with great success.
This process also cuts a little into the FR4 around the pad, as one wants to
make sure the complete pad is bare and therefore one has to overscan the
area to be cleaned.
If you like you can contact me off-line to get more details.

Regards,
Ahne Oosterhof,
Fine Line Stencil / A-Laser, Inc.
Beaverton, OR
503-641-9428



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, 20 April, 2006 14:18
To: [log in to unmask]
Subject: [TN] Parylene Coating Removal...

Hi All!

I've always thought that when it comes to removing parylene coating, about
the only way you can remove it is with some sort of mechanical means, i.e.;
microabrasion, or scraping. Burning through it with a soldering iron when
trying to do rework it is very, very difficult...I've tried it...it doesn't
work well at all.

I was just told that a chemical that I haven't heard of before might work,
it's called THF, or Tetrahydrofuran. I was told that it won't dissolve the
coating, but will cause it to lift from the PCB where it can be brushed
away. Have any of you ever heard of this stuff? I'm not a chemist, and I'm
not about to use it until I learn more about it.

The issue that I have is with a little tiny assembly that has been built and
parylene coated with some bad programmable hall effect switches installed.
The board is so small, and there are other components installed really close
to where the coating has to be removed. I'm afraid of getting them
microblasted because I'm afraid of damaging the other components. See the
assembly at:
http://stevezeva.homestead.com/files/8001_assy_backside.JPG ...the small
components are 0402's, so that gives you a visual scale of how big the
assembly is...

I've got the information in to a company that I found that does laser
ablation to remove coatings to give us a quote, so I'm waiting on that.
But if that turns out to be really expensive, I was contemplating using the
THF as plan "B" (provided the stuff will work and it doesn't hurt anything
else on the assembly).

Kind regards,

-Steve Gregory-
Senior Production Engineer
OAI Electronics
East 12th Street
Tulsa, Oklahoma 74112

(918) 836-9077 Ext.-507
(918) 706-2779 CELL

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2