Bev,
As the law is written (solder >85% Pb), I would argue that 100% Pb should be
exempt. Unless they were to instate a maximum Pb level (such as greater
than 85% and less than 98%), 100% Pb is greater than 85% and therefore
should be exempted. If someone were to argue against this, I would ask:
1. Is 95Pb/5Sn exempted? I think everyone would say yes.
2. 98Pb/2Sn?
3. 99Pb/1Sn?
4. 99.9Pb/0.1Sn?
5. 99.99Pb/0.01Sn?
At what level does it become not exempt?
The only thing that I see being a potential issue is that the term "solder"
is often defined as an ALLOY used to bond two metal surfaces. Since 100% Pb
is not an alloy, I see this as a potential sticking point. However, I am
sure that your 100% Pb has some impurities in it, so you are really
soldering with an alloy of 99.8Pb/0.05Sn/0.05Sb/0.1Bi (or whatever the
composition really is).
Best Regards,
Tim Jensen
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Monday, April 24, 2006 8:01 AM
To: [log in to unmask]
Subject: Re: [LF] Interpretation regarding high lead solders and RoHS
Thanks, Dave, other than a question from someone else, you are the only
other one to respond. However, my original question still stands: can
100% lead be considered a high lead solder to claim the exemption?
Obviously if it is not being used as a solder, I can see the answer
being no, but in the case I have stated...
Bev
RIM
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of MA/NY DDave
Sent: April 24, 2006 12:48 AM
To: [log in to unmask]
Subject: Re: [LF] Interpretation regarding high lead solders and RoHS
Hi Bev, JohnB, IPC LF Listservers,
http://listserv.ipc.org/scripts/wa.exe?
A2=ind0604&L=leadfree&D=0&T=0&X=51A2A101E52D6FE17F&[log in to unmask]&P=
1608
9
Bev, I have no idea what you are working on.
Those guys/gals at RIM are tricky people.
YET soldering isn't a key word to any EU Directive.
The application, or product, and customer is important.
If it falls under an EU directive, Lead (Pb) is a restricted material
with
as you noted certain exemptions and yahdah, yahdah.
Yours in Engineering, Dave
YiEngr, MA/NY DDave
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|