Ulrasonic welding is routinely done at a chip packaging level onto FR4
substrates.
However we're talking 1 'thou diameter gold or aluminium wires. I believe
the weld is made onto Ni/Ag plated pads.
Regards,
Eric Christison
Mechanical Engineer
Home, Personal, Communication Sector - Imaging Division
STMicroelectronics
33 Pinkhill
Edinburgh
EH12 7BF
Tel: +44 (0)131 336 6165
Fax: +44 (0)131 336 6001
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
> Sent: Friday, March 31, 2006 6:38 PM
> To: [log in to unmask]
> Subject: Re: [TN] Ultrasonic Weld to PCB with Ni Pads
>
>
> Not tried that one myself, couple of things though, the
> ultrasonic energy is going to have to have a sideways vector
> to "scub away" oxides. I am not sure if the systems normally
> used will do this or not.
>
> Second point is I recall that those ultrasonic welding
> systems rely on a Z axis force, and I am not sure what this
> will do to the shape/integrity of your FR4 PCB.
>
> TRY IT..............................
>
> John
>
> John Burke
> Senior Manager - Operations , Optichron [log in to unmask]
> W: 510 249 5233
> M: 408 515 4992
> http://www.optichron.com
> Profile: https://www.linkedin.com/e/fps/2665502/
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Rodney Miller
> Sent: Friday, March 31, 2006 6:32 AM
> To: [log in to unmask]
> Subject: Re: [TN] Ultrasonic Weld to PCB with Ni Pads
>
> Anyone, anyone, Bueller, Bueller....
>
> I think this will work, but I'm interested if anyone has
> applied this to PCB before?
>
> -----Original Message-----
> From: Rodney Miller [mailto:[log in to unmask]]
> Sent: Wednesday, March 29, 2006 10:06 AM
> To: 'TechNet '
> Subject: Ultrasonic Weld to PCB with Ni Pads
>
>
> I have a component with Nickel lead, a battery, and
> soldering/tinning it has been troublesome.
>
> I want to Ultrasonically Weld the leads to the PCB. Can I do
> this with PCB FR4 Material. I was thinking if I cannot do it
> through the PCB laminate, I might add a Via in pad and fill
> the via with Nickel plate.
>
> The laminate is .030 and the finish option on the pads would
> be Selective Immersion Ni, plated up to ???? 10um Maybe?
>
> Any input appreciated....
>
> Rodney L. Miller
> Tri-onics Inc
> Highland / Shanghai
>
> Integrity and Solutions for Electronic Outsourcing
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV
> 1.8e To unsubscribe, send a message to [log in to unmask] with
> following text in the BODY (NOT the subject field): SIGNOFF
> Technet To temporarily halt or (re-start) delivery of Technet
> send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|