Hi "WTHAYER,"
Yes, using low-CTE PCBs can be a solution to SJ reliability problems for
large ceramic components, particulalrly when done in combonation with large solder
joint heights [high-melt solder balls, solder columns] or conpliant leads.
But as you point out, you may be trading for other issues.
Werner
In a message dated 4/28/06 14:26:20, [log in to unmask] writes:
> If you HAVE TO use parts like that, try a low CTE PCB material, such as
> Arlon 85NT. This is nice stuff, with a listed CTE under 10ppm/C. It goes up a
> bit with high copper loading. Very stable, Tg over 200C, but sucks up
> moisture and is hell to board route without the edge fuzzing due to the aramid
> fibers.
>
> >>> [log in to unmask] 4/28/2006 1:47:58 pm >>>
> Hi Ioan,
> Castellated ceramic leadless chip carriers were a bad idea when the were
> developed in the '80s, and nothing has changed*oops, I forgot about that
> SAC-stuff
> making things worse.
> The problem is not the 'castellations' per se, but the fact that they will
> not allow the CC to swim up. Thus, the solder joint thickness is at a
> minimum,
> producing the worst-possible SJ reliability geometry--if you shim up the CC
> to
> increase SJ height, you can get about the same as what you get with BGAs
> with
> the same ball dimension.
> Putting large ceramic components on FR-4, castellated or not, is not a good
> idea.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
>
|